Stainless Steel - grade - EN 1.4876 - AISI 800H - UNS N08810 - DIN X10NiCrAlTi32-21
-
-
EN
1.4876
-
AISI
800H
-
UNS
N08810
-
DIN
X10NiCrAlTi32-21
-
Structure
Austenitic, creep-resistant
Composition
- C: 0,35-0,45%
- Cr: 14,0-16,0%
- Mn: max. 0,60%
- Ni: 13,0-15,0%
- P: max. 0,040%
- S: max. 0,030%
- Si: 1,50-2,50%
- Balance: W 2,00-3,00%
Applications
- Plant manufacturing
- Machine engineering
- Power generation
- Powerplant
Application
- Heat exchangers handling sulphuric acid and phosphoric acis contaminated by chlorides and flourides